Open Root Pipeline Welding With an E6010 Electrode

Doing an open root pipeline weld with an E6010 electrode needs 3 actions:

  1. Ensure the pipeline joint is fit up appropriately.
  2. Set your welding device right.
  3. Utilize the best welding technique.When it concerns doing an open

    root welds on pipeline or plate the basic guideline is you should have a great fit up! That is over half the fight. Even the very best welders will have a great deal of problem putting in the root pass if the joint fit up is bad. The perfect fit up must have a landing varying in between 1/16"to 1/8 of an inch. The space in between the 2 pipelines ought to likewise be in between 1/16"to 1/8 of an inch. Preferably you desire the landing and space to be constant all the method around the pipeline. It's simpler stated than done!Setting up of the welding device can be performed in 2 methods. The very first is following the electrodes produce's suggested amperage variety for that electrode. For putting in a root pass with an E6010 you have to begin in the extremely low end of the suggested amperage setting. From there you have to run a brief bead on the root so that you can modify the amperage setting till it is perfect.|From there you require to run a brief bead on the root so that you can modify the amperage setting till it is simply. The 2nd method is done by taking a piece of scrap metal and setting the welder simply hot sufficient to hardly bond without sticking. The 2nd method is how I prefer to establish my device and it generally get the device set perfect without needing to modify it to numerous times.The welding method utilized with an E6010 electrode on an open root pipeline weld is constantly a whipping movement. The only thing that

    truly alters with this method is for how long your whipping movement is. It can vary from going back and forth as much as one inch to as little simply as a shake of the electrode. The technique to obtaining a great root penetration is all in the keyhole. When you strike the arc you have to open a keyhole and keep your arc within it.|The space in between the 2 pipelines ought to likewise be in between 1/16"to 1/8 of an inch. Preferably you desire the landing and space to be constant all the method around the pipeline. The 2nd method is how I like to set up my device and it generally get the device set simply right without having to modify it to numerous times.The welding method utilized with an E6010 electrode on an open root pipeline weld is constantly a whipping movement.

Back to Top